Alloys: ZA-27 (ZA27, ZL2720, ZnAI27Cu2)
View
This toothed wheel consists of two parts which are assembled with cast-in spigots and bolts in special steel. The parts are made in zinc alloy ZA-27, and apart from trimming, receive no machining or other finishing operations. The part is produced in two sizes, the...
View
Die casting the three components in ZA-27 alloy offers good aesthetics and a near-net shape, which eliminates machining costs. At the same time, ZA-27 alloy provides good wear and bearing characteristics.
View
The goal of product designers for the 1/4 in. air ratchet was to lower product manufacturing costs while improving performance and appearance. The original product design specified an axial assembly–a machined steel head attached by a lock nut to a housing...
View
Engineers decreased time-to-market by utilising existing gear housing tooling to develop a higher load winch. Superwinch’s 1,500-lb. unit incorporated two 380 Aluminium die cast housings which functioned as rotating and stationary ring gears. By substituting...
View
Key material requirements for the office bundling machine are hardness and strength, the ability to hold good tolerances, and lubricity. ZA-27 was selected as the die casting material because of its hardness, strength, dimensional stability and natural lubricity. By...