Zinc die casting was chosen to reduce cost of an antenna base for mobile radio equipment, which originally a brass screw-machined part. Powder metallurgy was evaluated, but couldn’t achieve the required undercuts without machining. Zamak 2 alloy was specified to...
gearbox2_photo2_caseID129

Miter Gear Box – Hunter Douglas Venetian Blind

View

A four-piece miter gear assembly utilized zinc die casting for strength and precision. Both pinion gear shafts and housing halves are die cast net-shape, achieving full functionality without a cost penalty compared to alternative designs (thermoplastic housing/gears...
mirrorb2_photo2_caseID117

Mirror Bracket

View

The rigidity of the part ensures the quality of retro-vision due to the absorption of the vibrations compared to engineering plastics. Note the (omega) shape for the rigidity of the assembly. Rigidity inside the envelope (volume) and reduced width of the assembly,...
microwa2_photo2_caseID177

Microwave Guides (5 configurations)

View

Wave guides are built to exacting specifications in dimensional accuracy, straightness and flatness. Hot chamber die casting enables critical cavity sections to be cast with little or no draft; very difficult in aluminium cold chamber die casting. Flatness tolerance...
lasermt2_photo2_caseID107

Microscan Systems – VS 310 Scanner

View

Designers of an ultracompact scanner needed to reduce the internal envelope. The optics bracket was one component that was reduced in size but increased in functionality. The goal was design a single mounting bracket that would accommodate a laser module, a rotating...