The part : This high performance self-drilling insert for plaster board (partition, lining, ceiling) is always delivered with its self-tapping screw, forming two parts. The insert is composed of two rigidly attached and then articulated (body and toggle) and is...
Elta’s faucet construction is known as shell technology. It features a die-cast zinc cover, or escutcheon, over a brazed copper and brass assembly. The thin zinc cover is much more uniform than brass; it provides near net shape die casting with tolerances of 0.005...
das Gussteil ist Teil einer Baugruppe für einen mechanischen Türöffner, der mit dem Fuß bedient wird. Berührungslose Türöffnung ist beispielsweise in Krankenhäusern oder öffentlichen Sanitäranlagen unter hygienischen Aspekten ein Gewinn. Der Einbau erfolgt in...
The zinc pressure diecast corner stake fastened with pop rivets, fits tightly into the galvabond roll form section of the door. It has to compete with plastic moulded, aluminium extruded and aluminium pressed parts and does so because of the many properties of the...
Alloy 3 was chosen as the end cap material because of the ease with which it is processed. Both material and tooling cost are minimised and the product can be made with existing expertise and plant equipment. Alloy 3 castings can be produced with high dimensional...
Zinc diecast pillars support two different heights of floor system. The first is a low height (60 – 100mm) system for cables only, the second is higher (300 – 400mm) , used for air ducts under the floor. Zinc diecastings are designed for maximum strength....
One model of a range of decorative door handles. Zinc is used because of its ability to easily take a plated finish and because it can be cast to accurate dimensions.
A worm/helical gear set operates the linkage attached to the roof window frame. Originally, the helical gears were machined from brass, reinforced with a formed steel insert and installed with a plastic washer/spacer. The assembled gear’s cost became a factor...
To meet market requirements, Medeco wanted to develop a new high security lock priced just below its top-of-the-line dropbolt lock. The high-end lock model is all brass. The housing cover is investment cast and the thumbturn is a machined extrusion. As other processes...
The main feature of this lock design is that the handle is cast with a cylindrical shaped wall, but is then post formed to a spherical shape. If the Alloy 3 used for this casting did not have high ductility, the final shape could not be achieved and the pressure...
A four-piece miter gear assembly utilized zinc die casting for strength and precision. Both pinion gear shafts and housing halves are die cast net-shape, achieving full functionality without a cost penalty compared to alternative designs (thermoplastic housing/gears...
The initial design brief for the slave lock was that it had to have suitable mechanical properties to meet security door standards, have minimum design complexity and use the most logical material for the purpose. Initially a hybrid construction was considered, using...
Special features: precise recording, splash water protection for installation components, ensuring a circumferential wall fitting, uniform mold filling at heterogeneous wall thicknesses, short delay part : structurally specified wall thickness differences required...