cupcove2_photo2_caseID130

Cup & Cover of Gas Expander

View

Application with confirmed reliability since 40 years and always as performant with the evolution of the requirements. Performance of the process to realize and assemble pressure tight parts under 300 mba à 5 bars, with a lifelength of dies 5 times longer compared to...
doorbra2_photo2_caseID166

Door Brake

View

Automatic closing mechanisms for swing doors have to be adjustable and brake the movement of the door. The mechanism must be strong, resistant, reliable and compact enough to be housed in a casing. Pressure injected zinc alloy casings offer undeniable advantages such...
ima02

Doppelscharniergelenk

View

Doppelscharniergelenk “C-Hinge” als Türscharnier für Waschmaschine mit erweitertem Öffnungswinkel. Das bislang eingesetzte Stanzbiegeteil konnte durch das günstige Warmkammerverfahren wirtschaftlich darstellbar durch ein Zinkdruckgussteil ersetzt werden,...
electri2_photo2_caseID133

Electrical Auxiliary Switch Cam

View

A starter for large horse-power motors incorporated a fabricated sheet-metal cam bolted to a bracket, and welded to a shaft. Simplifying manufacturing and reducing cost, the cam design was changed to a single-piece ZA-12, graphite permanent mould casting....

Flansch

View

Den ersten Platz in der Kategorie „Konstruktion und Formenbau“ belegt die Kaspar Lüther GmbH & Co. KG. Bei dem von der Jury ausgezeichneten Flansch handelt es sich um ein Teil einer Baugruppe im Mahlwerk eines Kaffeevollautomaten. Durch die sehr enge Form- und...
handlel2_photo2_caseID84

Handle and Lock Assembly

View

In both residential and commercial construction projects, architects are frequently asked to design large windows and sliding glass doors. Sliding doors must be easy and comfortable to operate from either inside or outside and it must be possible to lock them. Zinc...
ima03

Housing for KitchenAid Coffee Machine

View

The 9,5 kg zamak housing of this designer coffee machine is  made from 8 zinc pressure die cast parts with weights between 2,2 kg and 75 gr. The parts are powder coated. To avoid any bubbles during thermal curing of the paint, the parts are vacuum cast to avoid gas...
leadscr2_photo2_caseID97

Lead Screw

View

Field problems with a gear-driven lead screw assembly prompted the company’s engineers to re-evaluate the design. The gear drive comprised a steel screw-machined shaft and a plastic gear. Assembly required the plastic gear to be pressed onto the shaft. Failures...
ima08

LEO Easy Opener

View

This design opener can open all kind of bottles without any damage and with  very little effort. With its innovative patented mechanism , this tool won the Bundespreis 2016 award in Germany. Reasons for choosing zinc alloy: ZP5 was chosen over other materials for its...
lightfi2_photo2_caseID99

Light Fittings

View

Zinc alloy pressure die castings in alloy Z 410 (BS1004B) are used to produce a wide range of light fittings varying from small individual lights, to multi-light chandeliers. A selection of lights shown here, ranging from small bronze plated lights, gold plated...
hub2_photo2_caseID110 (1)

Peerless Pull-Out Faucet – Delta

View

Initially, the hub–two intersecting cylinders–was a brazed assembly. Cylinders were screw machined from solid brass. Operations included turning, drilling, internal milling, cut-off and rolling of one cylinder end to accept a plastic transition piece. The...
structu2_photo2_caseID152

Structural Components

View

The KitchenAid mixer utilises zinc die castings for all of its structural components–the 4-1/2-quart pedestal model incorporates seven zinc castings and the 5-quart bowl support model incorporates eight zinc castings. Zinc castings provide a number of design...
tablewa2_photo2_caseID123

Tableware

View

Zinc die casting can help to create a gracious atmosphere for entertaining, when used in the form of prestige tableware, where good shape and meticulous finish are both important. The wide range of excellent surface finishes rely on both the experience of platers and...
toothed2_photo2_caseID154

Toothed Wheel

View

This toothed wheel consists of two parts which are assembled with cast-in spigots and bolts in special steel. The parts are made in zinc alloy ZA-27, and apart from trimming, receive no machining or other finishing operations. The part is produced in two sizes, the...