Low-Speed, High-Load Bearings

View

The Champion Series IV grader incorporates ZA-12 alloy low-speed, high load bearing to improve operation performance. Front Axle Bearings — This bearing application materialised as a replacement for the grader’s front axle needle bearings. The needle...