There are 8 studies matching your search criteria.

frameho2_photo2_caseID114

Frame Housing and Five Additional Mechanical Components

View

Key material requirements for the office bundling machine are hardness and strength, the ability to hold good tolerances, and lubricity. ZA-27 was selected as the die casting material because of its hardness, strength, dimensional stability and natural lubricity. By...
gearho2_photo2_caseID138

Gear Housing

View

Engineers decreased time-to-market by utilising existing gear housing tooling to develop a higher load winch. Superwinch’s 1,500-lb. unit incorporated two 380 Aluminium die cast housings which functioned as rotating and stationary ring gears. By substituting...
handgri2_photo2_caseID82

Hand Grinding Machine (Georges Renault)

View

Due to its realiability it allows the mounting of a precision bearing of an air turbine with a bevel gear. Allows the plastic overcoating Strength with precise shapes and thread with repetion at each production.
housinb2_photo2_caseID90

Housing and Base Plate

View

Originally the housing and base plate frame were sand cast aluminium and finish machined. Machining and assembly time took 3.5 hours per unit. During a redesign, the company set about to reduce costs without sacrificing quality or performance. This led to graphite...
lowspee2_photo2_caseID103

Low-Speed, High-Load Bearings

View

The Champion Series IV grader incorporates ZA-12 alloy low-speed, high load bearing to improve operation performance. Front Axle Bearings — This bearing application materialised as a replacement for the grader’s front axle needle bearings. The needle...
reducto2_photo2_caseID147

Reductor

View

The part is required to withstand mechanical strongh, precision in the bearing housing. Precision, Mechanical resistance and reliabilities Precision, Mechanical resistance, reliability.
strapad2_photo2_caseID186

Strap Adapter, Entry Slide Mount, Belt Sheave

View

Die casting the three components in ZA-27 alloy offers good aesthetics and a near-net shape, which eliminates machining costs. At the same time, ZA-27 alloy provides good wear and bearing characteristics.
toothed2_photo2_caseID154

Toothed Wheel

View

This toothed wheel consists of two parts which are assembled with cast-in spigots and bolts in special steel. The parts are made in zinc alloy ZA-27, and apart from trimming, receive no machining or other finishing operations. The part is produced in two sizes, the...