Sélecteur d’examples de pièces coulées en alliage de zinc



There are 2 studies matching your search criteria.

drivede2_photo2_caseID132

Drive Beck

View

The drive deck for Cherokee’s 5-1/4 in. WORM optical drive utilises a ZA-12 graphite permanent mould casting. From the start, graphite permanent mould was the process of choice because of its economical tooling cost, good dimensional control and low-volume...
structu2_photo2_caseID152

Structural Components

View

The KitchenAid mixer utilises zinc die castings for all of its structural components–the 4-1/2-quart pedestal model incorporates seven zinc castings and the 5-quart bowl support model incorporates eight zinc castings. Zinc castings provide a number of design...