ima01

Automotive Shift Level

View

This shift lever connects the shifter and the gear in ZF automotive gearboxes. This part  was originally an aluminum cast part but required tapping and other secondary operations to meet the close tolerances. Thanks to the  to close collaboration with the customer,...
ima06

Caster Housing

View

Part cast with Zincopor(R) technology which resulted in a weight reduction of 25%. With an annual production rate of 235,000 part/year, this represents a 10 tonnes reduction of zinc alloy.
ima04

Centrale Console

View

Key benefits: Outstanding control of each step and parameters involved in the full process i.e. from design to final part to achieve “the perfection” Same surface quality and appearance obtained on all the 6 cast parts of this assembly Fingers print surface free !!...
ima14

Electronic Connector

View

Key benefits: Close cooperation between diecaster and customer : clipping system Modern assembling technology : no screw = no creep!! This excellent product is the result of the perfect  knowledge of tooling and casting
ima07

Gear Knob AMG (Mercedes)

View

This casting part was originally produced in die-cast aluminum. It could be produced only with disproportionate effort and high scrap rates. The parting plane in the casting could never reach the surface quality standards because at that position was a vacuum...
ima07

High Tension Cage

View

The part is a device component warranting the operators security during the intervention on high-tension lines. Reasons for choosing zinc alloy: Complex tool design Combination of thin wall casting and rigidity Dimensional requirements e.g. internal and external...
jewelle2_photo2_caseID95

Jeweller’s perfume

View

The most famous Parisian jeweller, “”Boucheron””, has created a perfume, with a particularly outstanding design of bottle – an enlargement of a ring. The blue cap symbolises a cut stone whilst the bottle itself is supported in a fine...
motorch2_photo2_caseID118

Motor Chassis

View

This chassis for a motor drive unit for an automatic opening roller door was made from several pressed metal parts prior to being designed as a zinc diecasting. Diecasting in zinc alloy 3 provided the following benefits: 1.) Additional features such as pockets, the...
perfume2_photo2_caseID111

Perfume Vaporizer for Hand Bags

View

The part : This set of six parts, four of which are made of Zamak, makes up a rechargeable perfume vaporiser. The manufacturing : Some characteristics of the final product : – complexity of the assembly compared with the available space, – combination of...
ima06

Subframe and Carriage

View

The 3 parts form a subassembly that allows measuring the thickness of ophthalmic lenses before edging. The frame ensures the palpate lever guidance in the ophthalmic glass machine tool. Then, the glass is machined with the contour note during the palpate operation....
toothed2_photo2_caseID154

Toothed Wheel

View

This toothed wheel consists of two parts which are assembled with cast-in spigots and bolts in special steel. The parts are made in zinc alloy ZA-27, and apart from trimming, receive no machining or other finishing operations. The part is produced in two sizes, the...
ima11

Traffic Light Housing

View

The 2 parts are used as casing including and protecting the electric system of traffic lights. The material properties provides protection against vandalism and have much longer lifetime than polymer materials and due to thinner sections, lighter than the previous...