Sélecteur d’examples de pièces coulées en alliage de zinc



There are 9 studies matching your search criteria.

ima08

Central Support Unit

View

Central support unit for mounting all optical, electrical and mechanical components for the imaging plate technology in use in dentistry. In medical technology, die-cast zinc is used for many years. Overall, however, this area of ​​application is less known. The...
4a2_photo2_caseID135

Foot Switch – Control International

View

Over time, the costs associated with machining the cast-iron switch cover eroded manufacturing margins. The decision was then made to zinc die cast the cover. Zinc had the density and weight Conntrol International specified, and it provided better fit, better quality...
ima07

High Tension Cage

View

The part is a device component warranting the operators security during the intervention on high-tension lines. Reasons for choosing zinc alloy: Complex tool design Combination of thin wall casting and rigidity Dimensional requirements e.g. internal and external...
lowspee2_photo2_caseID103

Low-Speed, High-Load Bearings

View

The Champion Series IV grader incorporates ZA-12 alloy low-speed, high load bearing to improve operation performance. Front Axle Bearings — This bearing application materialised as a replacement for the grader’s front axle needle bearings. The needle...
plate2_photo2_caseID140

Plate

View

The part is machined on guiding bores and reference faces. Substitution to the pressed steel plate, due to high precision realized on machined diameters Ø < 0.02 mm obtained for a better cost.
ima06

Subframe and Carriage

View

The 3 parts form a subassembly that allows measuring the thickness of ophthalmic lenses before edging. The frame ensures the palpate lever guidance in the ophthalmic glass machine tool. Then, the glass is machined with the contour note during the palpate operation....
ima09

Support Unit for Drive

View

Segment drive for imaging plate technology in use in dentistry. The casting reveals a complex and accurate design tool. A modern and advanced die casting enables precise and optimum shape design that is consistent with the mechanical properties of the die-cast zinc...
ima11

Traffic Light Housing

View

The 2 parts are used as casing including and protecting the electric system of traffic lights. The material properties provides protection against vandalism and have much longer lifetime than polymer materials and due to thinner sections, lighter than the previous...