Casting Study: Cigarette Lighter Case

Major Selection Criteria: Decorative, Good Finish
Alloy: —
Application Field: Leisure & Sports
Application Size: Medium
Surface Finish: —
Casting Technique: Pressure Die Casting
Source: Seam

cigaret2_photo2_caseID75This series of cigarette lighters consists of a range of different models, each of which appeals to the individual taste of the user. The most prestigious models are given appropriate names – Golf, Nantes, Macito, Connubio, Mississipi, Gigolò, … The thickness of the zinc alloy pressure die castings forming these cases varies from 0.7 to 1 mm, giving weights of 30 to 60g. Each model has a different decoration on the external surfaces, and this is enhanced by the range of plated finishes–copper, brass, bronze, nickel, gold, …