Casting Study: Blackplate support pad for pin printer

Major Selection Criteria: Dimensional Precision, Mechanical Properties
Alloy: —
Application Field: Business/Office Equipment
Application Size: Medium
Surface Finish: —
Casting Technique: Pressure Die Casting
Source: Leibfreid Metallwerk AG

blackpl2_photo2_caseID68Modern printers require a pin support which must be cast pore free, non-deformable and of precise dimensions. Because of the large numbers of units produced, the life of the die is a determining factor. From the client’s point of view the sound dampening qualities of zinc castings is an important consideration, to ensure quiet operation of the printer. The striking surface is coated with a plastic film, so further surface treatments are unnecessary. The much longer die life was a particular advantage for zinc over aluminium die casting.