Casting Study: Cup & Cover of Gas Expander
Applicati
on with confirmed reliability since 40 years and always as performant with the evolution of the requirements. Performance of the process to realize and assemble pressure tight parts under 300 mba à 5 bars, with a lifelength of dies 5 times longer compared to the process of assembly with Aluminium. Easy crimping possibility for the alignment of the axles and levers, and the cup on the cover for demanding functional guarantee.