Casting Study: Gear Housing

Major Selection Criteria: Bearing Properties, Mechanical Properties, Net Shape
Alloy: ZA-27 (ZA27, ZL2720, ZnAI27Cu2)
Application Field: Automotive
Application Size: Rotating Gear: 3.5" x 5" dia.|Stationary Gear: 5-3/8" sq. x 2-1/8"
Surface Finish: Painted
Casting Technique: Pressure Die Casting
Source: Newton-New Haven Co., North Haven, CT

gearho2_photo2_caseID138Engineers decreased time-to-market by utilising existing gear housing tooling to develop a higher load winch. Superwinch’s 1,500-lb. unit incorporated two 380 Aluminium die cast housings which functioned as rotating and stationary ring gears. By substituting ZA-27 alloy for 380 Aluminium, the two new gear housings are cast in the original tooling but provide 2-1/2 times more strength. Without incurring additional tooling costs, Superwinch introduced a new 3,500-lb. winch. The superior performance of ZA-27 is in part due to the natural lubricity and high hardness of the alloy, which reduces friction and increases load capability and wear resistance.