Casting Study: Vise Components

Major Selection Criteria: Dimensional Precision, Mechanical Properties, Net Shape
Alloy: ZA-12 (ZA12, ZL1110, ZnAI11Cu1)
Application Field: Hand/Power Tools
Application Size: Medium
Surface Finish: Painted
Casting Technique: Gravity Casting
Source: Cash Mould and Castings Ltd., Hyde Park, Ontario

visecom2_photo2_caseID160Eight separate ZA-12 alloy castings are utilised in the TUCKER woodworking vise. Castings form the pivot block, front jaw, rear jaw, quick-release nut, yoke, stanchion, mounting plate and keeper plate. Based on the shapes needed to form the vise, casting easily became the metal forming process of choice, while ZA-12 alloy was chosen over cast iron for its greater strength and fluidity. Five reason are cited for choosing ZA-12 and graphite permanent mould casting: The ability to design features without machining or assembling; good dimensional control; quality control–the absence of hard spots, voids, distortions and warpage; good surface finish; and low tooling costs–25-30 percent less than sand casting patterns, match plates and tooling jigs.