Casting Study: Z Series Printers – Zebra Technologies

Major Selection Criteria: Complex Shape, Dimensional Precision, Other
Alloy: ZA-8 (ZL8, ZL0810, ZnAI8Cu1, alloy 8, ZA8)
Application Field: Business/Office Equipment
Application Size: 3-3/8 in. H x 3 in. W x 6 in. L
Surface Finish: As-Cast
Casting Technique: Pressure Die Casting
Source: Stroh Die Casting, Milwaukee, WI

platen3_photo3_caseID163The platen housing design incorporates three previous parts. In order to function properly, the material must be rigid and strong. The housing is cast with four elongated slots, four deep slots and seven cored holes, maximizing the need for structural support. In addition, the housing arm extensions are long and thin, susceptible to bending in a less rigid material. Diecast ZA-8 fulfills all design requirements by providing dimensional control, repeatability, strength and rigidity.