Casting Study: Spot Lamp Body

Major Selection Criteria: Good Finish, Thermal Conductivity
Alloy: —
Application Field: Electrical/Electronics
Application Size: Medium
Surface Finish: —
Casting Technique: Pressure Die Casting
Source: Bruschi S.R.L.

spotlam2_photo2_caseID151By using hot chamber pressure die casting for this product, Fos Nova SpA obtained excellent results both functionally and aesthetically, whilst saving production costs. Of special interest in this part is that the casting was fed through the central opening: this enabled a highly reflective surface to be obtained on the parabolic section of the casting without manual polishing. The excellent thermal conductivity of zinc, aided by thin cooling fins on the back surface of the casting enabled the heat generated in operation to be sufficiently dissipated, keeping temperatures within acceptable limits. Using pressure die casting also greatly simplified the machining required and the subsequent assembly operations, whilst maintaining the quality and effectiveness of the part.