Casting Study: Paper Feeding Guide for Thermic Printer

Major Selection Criteria: Corrosion Resistance, Dimensional Precision, Net Shape
Alloy: Zamak 5 (ZL5, ZL0410, ZnAI4Cu1, alloy 5)
Application Field: Industrial
Application Size: 80 x 30 x 1,2 mm / 3.15 x 1.18 x 0.05 inches
Surface Finish: Other
Casting Technique: Pressure Die Casting
Source: A.M.I. Fonderie

paperfe2_photo2_caseID109Anti-magnetic character of the Zinc Alloys, combined to the economy of the process wins over the press formed steel sheet and aluminium profiles.