Casting Study: Caster Housing Major Selection Criteria: Decorative, Good Finish, Light Weight, Mechanical Properties, Net Shape Alloy: Zamak 5 (ZL5, ZL0410, ZnAI4Cu1, alloy 5) Application Field: Business/Office Equipment Application Size: 100-250 g Surface Finish: As-Cast Casting Technique: Pressure Die Casting Source: Havelländische Zink-Druckguß GmbH & Co KG (Germany) Part cast with Zincopor(R) technology which resulted in a weight reduction of 25%. With an annual production rate of 235,000 part/year, this represents a 10 tonnes reduction of zinc alloy.
Casting Study: Caster Housing Major Selection Criteria: Decorative, Good Finish, Light Weight, Mechanical Properties, Net Shape Alloy: Zamak 5 (ZL5, ZL0410, ZnAI4Cu1, alloy 5) Application Field: Business/Office Equipment Application Size: 100-250 g Surface Finish: As-Cast Casting Technique: Pressure Die Casting Source: Havelländische Zink-Druckguß GmbH & Co KG (Germany) Part cast with Zincopor(R) technology which resulted in a weight reduction of 25%. With an annual production rate of 235,000 part/year, this represents a 10 tonnes reduction of zinc alloy.