Casting Study: Bearing Attachment

Major Selection Criteria: Dimensional Precision, Mechanical Properties
Alloy: Zamak 5 (ZL5, ZL0410, ZnAI4Cu1, alloy 5)
Application Field: Industrial
Application Size: Super Small
Surface Finish: —
Casting Technique: Pressure Die Casting
Source: Dru Meta-Metall GmbH & Co.

ln this example, a ball bearing housing which is die cast in alloy Z410 Bearing_attatchment(equivalent to BS 1004B) is attached to a thin continuously electrogalvanised steel sheet pressing. Studs – integral rivets – are cast into the housing and after the steel pressing is located, the five studs are simultaneously riveted onto the steel, giving a firm permanent joint.