Casting Study: Handle and Backplate Major Selection Criteria: Dimensional Precision, Good Finish, Integration of Multiple Functions Alloy: Zamak 3 (ZL3, ZL0400, ZnAI4, alloy 3) Application Field: Builders Hardware Application Size: 125 mm X 55 mm Surface Finish: Plated Casting Technique: Pressure Die Casting Source: Gainsborough Hardware Industries, Australia One model of a range of decorative door handles. Zinc is used because of its ability to easily take a plated finish and because it can be cast to accurate dimensions.
Casting Study: Handle and Backplate Major Selection Criteria: Dimensional Precision, Good Finish, Integration of Multiple Functions Alloy: Zamak 3 (ZL3, ZL0400, ZnAI4, alloy 3) Application Field: Builders Hardware Application Size: 125 mm X 55 mm Surface Finish: Plated Casting Technique: Pressure Die Casting Source: Gainsborough Hardware Industries, Australia One model of a range of decorative door handles. Zinc is used because of its ability to easily take a plated finish and because it can be cast to accurate dimensions.