Casting Study: Microprocessor Protection Housing
Part realized in large production volumes. Easy assembly with complex shapes, competing with pressed steel sheet. Zinc Castings’ superior thermal conductivity permits faster and greater heat dissipation provided by thinner radiating fins, complementing the repetitive and stable dimensional precision for the assembly of various components.