Casting Study: Quickclamp Air Prep System – IMI Norgren

Major Selection Criteria: Dimensional Precision, Good Finish, Mechanical Properties
Alloy: —
Application Field: Industrial
Application Size: 36.6 mm x 36.6 mm
Surface Finish: E-Coat/Powder Coat
Casting Technique: Pressure Die Casting
Source: IMI Norgren

quickclamp2_photo2_caseID182A newly designed air preparation system utilizes zinc die casting for the major components of the Quickclamp(TM) assembly (as well as the bodies, bowls and accessory parts of he filters, regulators and lubricators). Die cast zinc provided greater strength than molded plastic for this application and lower production costs that aluminum die casting because of net shape characteristics and longer die life. Other critical factors, which favor die-cast zinc, include its ability to maintain tight dimensional and flatness tolerances, low porosity and good finish.