Casting Study: Electronics Housing

Major Selection Criteria: Complex Shape, Dimensional Precision, EMI/RFI Shielding, Good Finish, Net Shape, Thin-Wall Construction
Alloy: Zamak 5 (ZL5, ZL0410, ZnAI4Cu1, alloy 5)
Application Field: Electrical/Electronics
Application Size: >250 g
Surface Finish: Other
Casting Technique: Pressure Die Casting
Source: Powercast Ortmann GmbH Co. KG (Geramny)

ima11SINAMICS Control Unit CU305 
The casting is a housing for the most demanding industrial electronics. To avoid short circuits it needs to be free of residual particles. To save costs  for post-processing and cleaning steps, a net-shape mold concept was developed. Moreover, the housing is a complex cast part with high difficulty. A requires high tolerance and accuracy  (near-net-shape). The length of the flow paths in relation to the wall thickness is a particular challenge.

Cast on 200ton machine, remove gate and overflows, CNC machining, grinding, glue the parts with rubber gasket, gluing the EMC seal.

Part size: 190 x 72 x 55 mm
Weight: 420g
Wall thickness: 1,5mm.