Casting Study: LEO Easy Opener

Major Selection Criteria: Decorative, Dimensional Precision, Good Finish, High Mass, Mechanical Properties, Net Shape
Alloy: Zamak 5 (ZL5, ZL0410, ZnAI4Cu1, alloy 5)
Application Field: Home Appliances
Application Size: 100-250 g
Surface Finish: Plated
Casting Technique: Pressure Die Casting
Source: Gross Druckguss Germany

ima08This design opener can open all kind of bottles without any damage and with  very little effort. With its innovative patented mechanism , this tool won the Bundespreis 2016 award in Germany.

Reasons for choosing zinc alloy:
ZP5 was chosen over other materials for its excellent surface finish, strength  and sense of quality.