Casting Study: Remote Control

Major Selection Criteria: Complex Shape, Decorative, Dimensional Precision, Good Finish, Mechanical Properties, Thin-Wall Construction
Alloy: Zamak 5 (ZL5, ZL0410, ZnAI4Cu1, alloy 5)
Application Field: Electrical/Electronics
Application Size: 100-250 g
Surface Finish: Plated
Casting Technique: Pressure Die Casting
Source: Haveländische Zink Druckguss (HZD) Germany

ima04This design high-end remote control has tactile control without any knobs. The zamak surface was cast to a thickness of 0,6mm with less than 0,05mm tolerance on thickness. Piezo elements translate the bending of the surface into electric signals. Casting of the part required all skills available. For casting this part, vakuum technology was used to eliminate any gas entrapment in the castings.

Reasons for choosing zinc alloy:
ZP5 was chosen over other materials for its excellent surface finish, strength, ability to cast very thin surfaces with extreme low tolerances and free of defects.